Views: 81567 Author: Site Editor Publish Time: 2026-11-20 Origin: Site
1. The Five Characteristic Temperatures of Polymers
In polymer science, three important temperatures are defined according to the state of the polymer molecular chains: the crystallization temperature, the melting temperature, and the decomposition temperature.
- Crystallization temperature: The temperature at which polymer molecular chains transform from an amorphous state to a crystalline state.
- Melting temperature (Tm): The temperature at which polymer crystals melt.
- Decomposition temperature (Td): The temperature at which a polymer decomposes into small molecules.
In addition, two important temperatures are defined according to the motion state of the polymer molecular chains: the glass transition temperature (Tg) and the viscous flow temperature (Tf). These two temperatures divide polymers into three states. When T < Tg, the polymer is in a hard solid state, the molecular chains cannot move, and the material has no processability. When Tg < T < Tf, the polymer is in a rubbery state; the main chains cannot move, but some side chains and pendant groups can move, and the polymer exhibits a certain degree of stretchability. When T > Tf, the polymer is in a viscous flow state, that is, a flowable state, which is generally the actual processing temperature of the polymer.
2. Amorphous Polymers and Crystalline Polymers
The five temperatures mentioned above require particular attention in polymer processing. However, different polymers exhibit different crystallization behavior and different characteristic temperatures owing to differences in functional groups, pendant groups, side chains, molecular helix structures, and other factors. Polymers can be divided into the following two categories according to crystallinity.
(1) Amorphous polymers
By definition, because their crystallinity is very low, the influence of crystalline structure on the polymer state is relatively small, and amorphous polymers do not actually have a specific melting temperature (commonly referred to as the melting point). Polymers such as PET and PC, whose molecular chains contain relatively large functional groups and numerous pendant groups and side chains, generally have low crystallinity and are classified as amorphous polymers.
(2) Crystalline polymers
Polymers with a crystallinity above 80% are referred to as crystalline polymers. Polymers such as PE and PP, which have simple repeating units, regular structures, and high symmetry, generally exhibit high crystallinity and are classified as crystalline polymers.
3. Why Is the Melting Point Often Regarded as the Extrusion Temperature?
In actual processing, the processing temperature of a polymer is mainly determined by its viscous flow temperature. At this temperature, the polymer exhibits overall flowability and can be processed by extrusion, injection molding, and other forming methods. Why, then, is the melting point of a polymer often regarded as its extrusion temperature in many cases? This question must be analyzed from the perspective of crystallization for both crystalline and amorphous polymers.
In amorphous polymers, the influence of crystalline structure on the polymer state is relatively small, and no specific melting temperature (melting point) exists. However, when the polymer state is characterized by differential scanning calorimetry (DSC), amorphous polymers also exhibit a melting peak. This melting peak actually corresponds to the temperature at which the molecular chains absorb sufficient energy to acquire overall mobility. Therefore, for amorphous polymers, the commonly referred to melting point is the viscous flow temperature at which the molecular chains transition from the rubbery state to the viscous flow state, and the polymer can be extruded near this melting temperature.
For crystalline polymers, the melting temperature and the viscous flow temperature are two different temperatures. Taking PP as an example, as mentioned in the previous article, the melting point of PP is approximately 165°C, while the extrusion temperature is usually set at approximately 220°C. This is because PP has high crystallinity. At the melting point, the crystals melt and transform from a crystalline state to an amorphous state. At this temperature, however, the PP molecular chains still do not possess flowability. The temperature must continue to rise to the viscous flow temperature so that the molecular chains receive sufficient energy to move. Therefore, the processing temperatures of highly crystalline materials such as PE and PP are considerably higher than their melting points.
Although increasing the temperature can provide better flowability, higher temperature is not always better. On the one hand, after the polymer reaches the viscous flow temperature, the effect of further temperature increases on improving flowability gradually diminishes, which represents wasted energy from an energy consumption perspective. On the other hand, the higher the temperature, the more easily the polymer undergoes degradation under the shearing action of the extruder screw, and it may even decompose into small molecules, adversely affecting product quality.
Understanding these thermal transitions is essential for selecting appropriate processing temperatures and maintaining stable product quality. Equally important is the use of well-designed screws and barrels that ensure uniform melting, reduce excessive shear, and minimize the risk of polymer degradation.
About SUPERIOR MACHINERY
Established in 1992, SUPERIOR MACHINERY has been engaged in the rubber and plastic molding machinery industry for more than 30 years. With an increasing market share, the company has established itself in the field of high-quality fully hardened screws and bimetallic barrels that are highly resistant to wear, corrosion, high pressure, and high speed. The company has a strong technical team composed of industry elites and professional consultants.
Since 2000, we have launched the Complete Machine Production Line, Dehumidification and Drying series, Material Conveying series, Hot and Cold Temperature Control series, Crushing and Recycling series, Material Mixing series, Automation Equipment, Molds, Accessories, and other products. We remain competitive in the market.
SUPERIOR MACHINERY pursues the ultimate quality of materials and products, and always looks forward to becoming your most trusted and reliable partner.
A large extruder can show higher melt temperature but lower melt pressure than smaller ones under identical settings, due to longer residence time, greater shear heat, and lower melt viscosity. Process parameters therefore cannot be directly transferred between extruders of different sizes.
This article explains why extrusion temperatures are usually set above a polymer's melting point. It reviews five characteristic temperatures and distinguishes amorphous from crystalline polymers. Amorphous polymers flow near their "melting" peak, while crystalline polymers such as PE and PP require heating above the melting point to reach viscous flow. Excessive temperature is discouraged because it wastes energy and increases degradation risk.
Injection molding is fundamentally a process of balancing driving force (pressure) and resistance (cavity pressure). During injection, cavity resistance changes continuously as the melt fills the mold, meaning injection pressure is never constant—even at a fixed speed. The article compares two control approaches: variable closed-loop systems, where injection speed dominates and pressure adjusts automatically, and open-loop proportional valve systems, where pressure and speed must be set manually and interact with each other. It concludes that multi-stage pressure settings are valuable for protecting molds and ensuring stable production, particularly in multi-cavity applications.
This article examines the relationship between injection stroke and screw length-to-diameter (L/D) ratio in injection molding machines. Because the screw retracts during plasticization, a longer injection stroke reduces the effective L/D ratio, creating axial temperature gradients that cause inconsistent melt temperature and uneven part quality—especially in multi-cavity molds. Increasing the L/D ratio improves mixing and reduces axial temperature variation. The article recommends limiting injection stroke to approximately four times the diameter of the B screw and concludes that long-stroke, low-L/D designs suit single-cavity products with modest quality requirements, while constrained stroke and higher L/D ensure multi-cavity product consistency.
This article explains the differences between A, B, and C injection-molding screws, which are distinguished primarily by diameter and length-to-diameter ratio. A-type screws offer high pressure and excellent mixing for engineering materials and precision thin-walled parts; B-type screws are the versatile default for over 70% of general-purpose plastics; C-type screws provide high capacity for large, thick-walled components. Three selection rules are provided: keep shot size within 30%–70% of screw capacity, choose fine high-pressure screws for transparent parts, and specify wear-resistant alloys for fiber-reinforced materials.
Screw cleaning is critical to product quality in modified plastics production, yet often overlooked. This article analyzes four common cleaning methods for twin-screw extruders—resin cleaning, disassembly and manual cleaning, flame cleaning, and water-based cleaning—covering their operational principles, key process steps, precautions, and limitations. It provides practical guidance for selecting and combining cleaning methods based on material characteristics, equipment condition, quality requirements, and cost-effectiveness, while emphasizing standardized operations and regular maintenance to extend equipment service life.
For PVC plastic extrusion production lines, feeding method selection depends on material form and process requirements. Three common systems are compared: spring feeders (quick to clean, suitable for frequent color changes but poor with high-filler powders), screw feeders (high flow rate and anti-bridging, ideal for high-filler powders but not for fiber-reinforced materials), and vacuum feeders (dust-free and closed-loop, best for cleanrooms and fiber reinforcement but limited at high output).