Views: 47843 Author: Site Editor Publish Time: 2026-11-16 Origin: Site
1. Introduction
In recent production, an unusual phenomenon was observed on a three-layer co-extrusion PE blown film line consisting of three extruders. Two skin-layer extruders are small machines with an L/D ratio of 20, while the central core-layer extruder is a large machine with an L/D ratio of 30. During production, the melt temperature of the large extruder was consistently higher than that of the small extruders, while its melt pressure was lower than that of the other two small extruders. For example, when the melt temperatures of the three extruders were close, the melt pressure of the central large extruder was slightly lower than that of the other two. Conversely, when the melt pressures of the three extruders were close, the melt temperature of the large extruder was 5–10°C higher than that of the other two, provided that the extrusion temperatures set on all three machines were identical. Relevant literature was reviewed and summarized, and the conclusions are presented below for discussion.
2. Material Transformations Inside the Extruder
Before discussing the causes, it is necessary to review the transformations that materials undergo inside an extruder. This is a complex process involving both physical and chemical changes, generally divided into the following stages:
2.1 Feeding and Conveying Stage
Feeding: Solid pellets or powder enter the extruder barrel through the hopper.
Conveying: Under the rotation of the screw, the material is conveyed forward along the screw. At this stage, the material exists mainly in solid form and moves forward through the screw channel.
2.2 Preheating and Melting Stage
Preheating: As the material moves along the screw, heating elements in the barrel, such as electrical heaters, and the shearing action of the screw begin to raise the material temperature.
Melting: When the temperature reaches the melting point of the material, the material begins to melt and gradually transforms from a solid into a viscous melt. This process usually occurs in the compression section of the screw.
2.3 Mixing and Plasticizing Stage
Mixing: Under the shearing action of the screw, the molten material is thoroughly mixed. Twin-screw extruders are particularly suitable for this stage owing to their high mixing capacity.
Plasticizing: Through screw shearing and mixing, the material reaches a uniform molten state and forms a melt with good flowability. This stage usually occurs in the homogenizing section of the screw.
2.4 Reaction Stage (Reactive Extrusion)
Chemical reaction: If the extruder is used for reactive processing, such as grafting, chain extension, or polymerization, chemical reactions occur in the molten state. These reactions require precise control of temperature, shear force, and residence time.
Modification: Through chemical reactions, the molecular structure of the material changes, thereby achieving material modification.
2.5 Forming Stage
Strictly speaking, this stage occurs in the die and is not a transformation within the extruder.
Forming: After sufficient mixing and plasticizing, the melt is formed through the die. The shape and design of the die determine the shape of the final product, such as pipe, sheet, or film.
Cooling: The formed melt must be cooled and sized through a cooling system, such as water cooling or air cooling, to prevent product deformation.
3. Causes of Temperature and Pressure Differences
A previous article discussed the differences between single-screw and twin-screw extruders. Since most large production extruders are single-screw machines, and the PE blown film equipment discussed here is also single-screw, this article focuses on single-screw extruders and examines the influence of extruder size on melt temperature and pressure. Based on the material transformations described above, the higher melt temperature and lower melt pressure of the large single-screw extruder can be attributed mainly to the following three factors:
The extruder is larger, so the residence time of the material inside the extruder is longer. This means that the material is subjected to shear and thermal effects for a longer period. Even if the set temperature is the same, the actual melt temperature will be higher.
The screw of a large extruder generally has a larger L/D ratio and is longer, so the shearing action on the material is more sufficient and the accumulation of shear heat is greater. This additional shear heat leads to an increase in melt temperature.
The melt viscosity of a polymer melt is negatively correlated with temperature; that is, the higher the temperature, the lower the melt viscosity. Because the large extruder provides more thorough shear and plasticizing, the material temperature increases, the melt viscosity decreases, and the flowability is enhanced. Consequently, the melt pressure is lower when the melt passes through the screen pack.
It can therefore be seen that small and large extruders are not related by simple proportional scaling. When the same material is processed on different extruders, the process parameters cannot be directly copied. When scaling up from laboratory research to actual production, differences in the melting and plasticizing efficiency of different equipment must also be considered. This is particularly important when screw configurations differ, as the melting and plasticizing effect on the material can vary considerably.
4. Summary
Configurations using one large and two small extruders in three-layer co-extrusion are common. A well-known example is biaxially oriented film production. Because the skin and core layers have different functions and required thicknesses, three-layer co-extrusion structures—whether ABA or ABC—often use a combination of large and small extruders. If the melt temperatures or melt pressures of different extruders are inconsistent or differ significantly, a velocity difference will exist when the melts converge in the die, leading to interlayer separation or apparent quality defects. Therefore, the temperature and pressure settings of extruders are not merely intended to ensure complete melting and plasticizing; they are process parameters worthy of attention and study.4. Summary
Configurations using one large and two small extruders in three-layer co-extrusion are common. A well-known example is biaxially oriented film production. Because the skin and core layers have different functions and required thicknesses, three-layer co-extrusion structures—whether ABA or ABC—often use a combination of large and small extruders. If the melt temperatures or melt pressures of different extruders are inconsistent or differ significantly, a velocity difference will exist when the melts converge in the die, leading to interlayer separation or apparent quality defects. Therefore, the temperature and pressure settings of extruders are not merely intended to ensure complete melting and plasticizing; they are process parameters worthy of attention and study.
Understanding these process differences is essential for stable production, and equally important is selecting screw and barrel components that deliver consistent melting and plasticizing performance across different machine sizes and configurations.
About SUPERIOR MACHINERY
Established in 1992, SUPERIOR MACHINERY has been engaged in the rubber and plastic molding machinery industry for more than 30 years. With an increasing market share, the company has established itself in the field of high-quality fully hardened screws and bimetallic barrels that are highly resistant to wear, corrosion, high pressure, and high speed. The company has a strong technical team composed of industry elites and professional consultants.
Since 2000, we have launched the Complete Machine Production Line, Dehumidification and Drying series, Material Conveying series, Hot and Cold Temperature Control series, Crushing and Recycling series, Material Mixing series, Automation Equipment, Molds, Accessories, and other products. We remain competitive in the market.
SUPERIOR MACHINERY pursues the ultimate quality of materials and products, and always looks forward to becoming your most trusted and reliable partner.
A large extruder can show higher melt temperature but lower melt pressure than smaller ones under identical settings, due to longer residence time, greater shear heat, and lower melt viscosity. Process parameters therefore cannot be directly transferred between extruders of different sizes.
This article explains why extrusion temperatures are usually set above a polymer's melting point. It reviews five characteristic temperatures and distinguishes amorphous from crystalline polymers. Amorphous polymers flow near their "melting" peak, while crystalline polymers such as PE and PP require heating above the melting point to reach viscous flow. Excessive temperature is discouraged because it wastes energy and increases degradation risk.
Injection molding is fundamentally a process of balancing driving force (pressure) and resistance (cavity pressure). During injection, cavity resistance changes continuously as the melt fills the mold, meaning injection pressure is never constant—even at a fixed speed. The article compares two control approaches: variable closed-loop systems, where injection speed dominates and pressure adjusts automatically, and open-loop proportional valve systems, where pressure and speed must be set manually and interact with each other. It concludes that multi-stage pressure settings are valuable for protecting molds and ensuring stable production, particularly in multi-cavity applications.
This article examines the relationship between injection stroke and screw length-to-diameter (L/D) ratio in injection molding machines. Because the screw retracts during plasticization, a longer injection stroke reduces the effective L/D ratio, creating axial temperature gradients that cause inconsistent melt temperature and uneven part quality—especially in multi-cavity molds. Increasing the L/D ratio improves mixing and reduces axial temperature variation. The article recommends limiting injection stroke to approximately four times the diameter of the B screw and concludes that long-stroke, low-L/D designs suit single-cavity products with modest quality requirements, while constrained stroke and higher L/D ensure multi-cavity product consistency.
This article explains the differences between A, B, and C injection-molding screws, which are distinguished primarily by diameter and length-to-diameter ratio. A-type screws offer high pressure and excellent mixing for engineering materials and precision thin-walled parts; B-type screws are the versatile default for over 70% of general-purpose plastics; C-type screws provide high capacity for large, thick-walled components. Three selection rules are provided: keep shot size within 30%–70% of screw capacity, choose fine high-pressure screws for transparent parts, and specify wear-resistant alloys for fiber-reinforced materials.
Screw cleaning is critical to product quality in modified plastics production, yet often overlooked. This article analyzes four common cleaning methods for twin-screw extruders—resin cleaning, disassembly and manual cleaning, flame cleaning, and water-based cleaning—covering their operational principles, key process steps, precautions, and limitations. It provides practical guidance for selecting and combining cleaning methods based on material characteristics, equipment condition, quality requirements, and cost-effectiveness, while emphasizing standardized operations and regular maintenance to extend equipment service life.
For PVC plastic extrusion production lines, feeding method selection depends on material form and process requirements. Three common systems are compared: spring feeders (quick to clean, suitable for frequent color changes but poor with high-filler powders), screw feeders (high flow rate and anti-bridging, ideal for high-filler powders but not for fiber-reinforced materials), and vacuum feeders (dust-free and closed-loop, best for cleanrooms and fiber reinforcement but limited at high output).